Iron Ore Fines (Sinter Feed – Fe content: 64,50% above)
Origin: Brazil and or other country (best choice of the seller)
Specification:
Guaranteed Specification:
Fe 64,50% rejection bellow 63,00%
Al2O3 6,69% rejection over 10,50%
SiO2 10,80% rejection over 13,50%
S 0,007%, max 0,03%
P 0,025%, max 0,06%
Physical Characteristics:
0.15-3mm 30%min
3-5mm 60%max
5- 10mm 10%max
Moisture 8.00% at 105 degrees C